中文摘要: 以刚果(金)科卢韦齐矿区氧化铜精矿为原料,在1500 ℃下采用高钙渣型开展1 h焦炭还原熔炼实验。研究表明:从提高铜回收率的角度来看,钙硅化(CaO/SiO2)为0.55比较适宜,当CaO/SiO2大于0.5时,铁的竞争性还原反应加剧,造成铜回收率与铜还原率差距加大。综合考虑, CaO/SiO2配料比选择0.50~0.55。炉渣黏度受O/Si变化和AlO5-4 补网作用的协同影响。
Abstract:With copper oxide concentrate from Kolwezi mining area in Congo (Kinshasa) as raw material, a 1-hour coke reduction smelting experiment was carried out with high calcium slag at 1500 ℃. The research shows that the CaO/SiO2 ratio of 0.55 is appropriate to improve copper recovery. When the CaO/SiO2 ratio is greater than 0.5, the competitive reduction reaction of iron intensifies, resulting in a larger gap between copper recovery and copper reduction. Based on comprehensive consideration, the CaO/SiO2 blending ratio is 0.50 ~ 0.55. Slag viscosity is affected by the change of O/Si ratio and AlO5 -4 Synergistic influence of network supplement.
文章编号:20221129002 中图分类号:TF811
基金项目:“十三五”国家重点研发计划项目(2019YFC1907304)
引用文本:
张磊,蒋开喜,谢锋,王伟,路殿坤.钙硅比对氧化铜精矿还原熔炼的影响[J].铜业工程,2023,(2):152-157